Welcome to Westonci.ca, where your questions are met with accurate answers from a community of experts and enthusiasts. Get immediate and reliable answers to your questions from a community of experienced experts on our platform. Explore comprehensive solutions to your questions from knowledgeable professionals across various fields on our platform.

A gear component (0.2% C) is carburized with C for increased hardness. By specification, a carbon concentration of 0.75% C is required at an 80 um depth. Calculate the time required (ir hours) at 1100°C with the gas surface concentration of 1.3 % C. D=5x10-13 m2/s. Show relevant steps how you arrived at the answer Comment on whether the suggested carburizing time of 3 hours is sufficient, also mention the calculated time in hours